Follow the RCA Clean method below with a hydrofluoric acid (HFA) wash to remove oxide layer. The oxide layer will take a few hours in a normal atmosphere to regrow so deposition of metal should proceed immediately after the HFA wash.<br><br>
 +
[[Media:RCA_Clean.pdf]]<br>
 
[[Media:Making_ohmic_contacts.pdf]]
 
[[Media:Making_ohmic_contacts.pdf]]

Latest revision as of 17:06, 22 May 2019

A Schottky Diode








- Useful Information -
Follow the RCA Clean method below with a hydrofluoric acid (HFA) wash to remove oxide layer. The oxide layer will take a few hours in a normal atmosphere to regrow so deposition of metal should proceed immediately after the HFA wash.

Media:RCA_Clean.pdf
Media:Making_ohmic_contacts.pdf